Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | -29.4 °C @Pressure 0.101 MPa |
-20.9 °F @Pressure 14.6 psi |
|
Shandong Dongyue Polymer HFP Hexafluoropropylene Usage: HFP is one of the important fluorinated monomer with high chemical activity. It can produce kinds of the fine chemical products, such as surfactant, medicine intermediate, 227EA for fire ex.. |