Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Softening Point = 98.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 98.9 - 104 °C
210 - 220 °F
Plaskolite Optix® DA Digital Acrylic Sheet
Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup..
Copyright © lookpolymers.com All Rights Reserved