Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 505 °C | 941 °F | |
Ferro EG 2992 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: SRRG Typical Application: Ferrites Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insu.. |