Thermal Properties Metric English Comments
Softening Point 465 °C
869 °F
Ferro EG 3608 Metal Sealing
Glass Type: Si-Ti Alkali Typical Powder Form: VSD Typical Application: Al Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals fo..