Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 86.2 °C | 187 °F | ETM 22-24 |
ExxonMobil ESCOREZ™ 5380 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, metallocen.. |