Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 455 °C | 851 °F | Permanent Softening |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Softening Point | 455 °C | 851 °F | Permanent Softening |
CMW® 353 Copper Alloy CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatm.. |