Polymer Property : Softening Point = 85.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 85.0 - 105 °C
185 - 221 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-530 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 85.0 - 105 °C
185 - 221 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-560 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 85.0 °C
185 °F
Kofler; ASTM D1525
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv..
Softening Point 85.0 - 95.0 °C
185 - 203 °F
Beijing Ranger Chem WSR604 Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 85.0 - 95.0 °C
185 - 203 °F
Beijing Ranger Chem 194 Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.