Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 815 °C | 1500 °F | 10<sup>7.6</sup> dPa-s |
Schott BOROFLOAT® Borosilicate Float Glass This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro.. |