Polymer Property : Softening Point = 77.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 25.0 - 32.0 °C
77.0 - 89.6 °F
Beijing Ranger Chem E-39-D Semi Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 25.0 - 29.0 °C
77.0 - 84.2 °F
Beijing Ranger Chem SM-E-39D Semi Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.