Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 73.0 - 75.0 °C | 163 - 167 °F | Average value: 74.2 °C Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Softening Point | 65.0 - 75.0 °C | 149 - 167 °F | Kofler; MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® DAP 750/2 Thermoplastic Polyurethane The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pelle.. |
|||
Softening Point | 65.0 - 75.0 °C | 149 - 167 °F | |
Beijing Ranger Chem 191 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 65.0 - 75.0 °C | 149 - 167 °F | |
Beijing Ranger Chem SM-601R Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 65.0 - 75.0 °C | 149 - 167 °F | |
Beijing Ranger Chem 0191S Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |