Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 660 °C | 1220 °F | |
Ferro EG 2927 Metal Sealing Glass Type: Sr-B-Al Typical Powder Form: VSD Typical Application: Comp. - Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched .. |
|||
Softening Point | 660 °C | 1220 °F | |
Ferro F 1040 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |