Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 645 °C | 1190 °F | |
Ferro EG 2807 Metal Sealing Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc.. |
|||
Softening Point | 645 °C | 1190 °F | |
Corning 0159 Lead Barium Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |