Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 580 °C | 1080 °F | |
Ferro EG 3600 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |