Polymer Property : Softening Point = 563 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 295 °C
563 °F
Valley Adhesives EM-105 High Performance Application Glue Stick
Valley Adhesives EM-105 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol..
Copyright © lookpolymers.com All Rights Reserved