Polymer Property : Softening Point = 560 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 560 °C
1040 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8532 Soft Glass
Soft glass, free from Na, of high lead content, lower sealing temperature than glass 8531, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information ..