Polymer Property : Softening Point = 513 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 513 °C
955 °F
Ferro CF 7586 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t..