Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 205 °C | 401 °F | |
Valley Adhesives EM-221 Low Temperature Application Glue Stick Valley Adhesives EM-221 Low Temperature Application Glue StickRapid strength build up to 0149; Excellent hot tack and wetting; Safe on styrofoam and heat sensitive materials; Bonds corrugated boxes .. |