Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | >= 1600 °C | >= 2910 °F | |
Zircar Ceramics RAHP Reticulated Alumina Hearth Post ZIRCAR Reticulated Alumina Hearth Posts are rigid highly porous rods and shapes of fine grain dense alumina ceramic. An off-shoot of superalloy casting technology from the aerospace industry, these .. |