Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 1583 °C | 2881 °F | Varies with thermal history |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |