Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 139.6 °C | 283.3 °F | ETM 22-24 |
ExxonMobil Oppera PR 100N (EU) Modifier Product Description: A performance modifier resin designed for use in blends with polymers.Availability: Africa & Middle East and EuropeInformation provided by ExxonMobil |