Polymer Property : Softening Point = 283.1 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 139.5 °C
283.1 °F
ETM 22-24
ExxonMobil ESCOREZ™ 5340 Petroleum Hydrocarbon Resin
The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A..