Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 137.7 °C | 279.9 °F | ETM 22-24 |
ExxonMobil Oppera PR 100A (AM) Modifier Product Description: A performance modifier resin designed for use in blends with polymers.Availability: Central America, South America and North AmericaInformation provided by ExxonMobil |