Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 130 - 150 °C | 266 - 302 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-573 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 130 - 150 °C | 266 - 302 °F | |
Beijing Ranger Chem 199 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 130 - 150 °C | 266 - 302 °F | |
Beijing Ranger Chem SM-1009 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 130 - 150 °C | 266 - 302 °F | |
Beijing Ranger Chem SM-609 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |