Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 260 °C | 500 °F | |
Victrex® Vicote® F813 Black Polyetheretherketone (PEEK) Liquid Dispersion VICOTE® is the brand name for the Victrex range of coatings. The VICOTE Coatings are available through Victrex plc or its preferred coater network. The VICOTE F813Blk grade has been specifically fo.. |