Polymer Property : Softening Point = 246.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 119.2 °C
246.6 °F
ETM E-24
ExxonMobil ESCOREZ™ 1401 (Europe) Petroleum Hydrocarbon Resin
ESCOREZ™ 1401 is a modified aliphatic hydrocarbon resin with a narrow molecular weight distribution and a high softening point. It is a tackifying resin designed to provide high temperature perform..