Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.Applications: genera.. |
|||
Softening Point | 93.7 °C | 201 °F | ETM 22-24 |
ExxonMobil ESCOREZ™ 1310 LC Petroleum Hydrocarbon Resin This product is a light colored, premium aliphatic hydrocarbon resin with narrow molecular weight distribution. It is designed to tackify a variety of adhesive polymers including EVA, metallocene .. |