Polymer Property : Softening Point = 178 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 178 °C
352 °F
Valley Adhesives EM-500 High Temperature Application Glue Stick
Valley Adhesives EM-500 High Temperature Application Glue StickHi and low temperature general purpose; Bonds P.O.P. displays, porous and non-porous substrates, paper, corrugated boxes, fabrics, and ..
Softening Point 178 °C
352 °F
Valley Adhesives EM-900 High Temperature Application Glue Stick
Valley Adhesives EM-900 High Temperature Application Glue StickGeneral purpose; Bonds P.O.P. displays, porous and non-porous substrates, paper, corrugated boxes, fabrics, and foams.