Polymer Property : Softening Point = 171 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 63.0 - 77.0 °C
145 - 171 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-660 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 63.0 - 77.0 °C
145 - 171 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-853 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..