Thermal Properties Metric English Comments
Softening Point 1700 °C
3090 °F
Saint-Gobain Quartzel® Fused Quartz Textiles
Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava..