Polymer Property : Softening Point = 1530 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 830 °C
1530 °F
Potters Industries Spheriglass® EMB-10 Low Alkaline Boro-Silicate Solid Glass Microspheres
Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.Information provided by Potters Industries.
Softening Point 830 °C
1530 °F
Potters Industries Spheriglass® EMB-20 Low Alkaline Boro-Silicate Solid Glass Microspheres
Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.Information provided by Potters Industries.
Softening Point 830 °C
1530 °F
Mo-Sci Corporation GL-0179 Borosilicate Glass Spheres
Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control,..
Softening Point 830 °C
1530 °F
Mo-Sci Corporation GL-0186 Borosilicate Glass Spheres
Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0186 beads include: high temperature spacer material for gauge control, coating, fil..
Softening Point 830 °C
1530 °F
Mo-Sci Corporation GL-0261 Ni Coated Borosilicate Glass Spheres
Appearance: Solid borosilicate glass microspheres with metallic nickel coatingTypical applications of GL-0261 glass microspheres include: conductive filler for plastic, pigment, and etc.Information ..
Softening Point 830 °C
1530 °F
Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres
Appearance: Solid borosilicate glass microspheres with metallic copper coatingTypical applications of GL-0263 glass microspheres include: conductive filler for plastic, pigment, and etc.Information ..
Softening Point 830 °C
1530 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8660 Borosilicate Glass
Borosilicate glass for sealing to tungsten, of high cesium content Red eye reduction flash for electronic flashbulbs, longer life in comparison with glass 8487 The heavy metal content for the elem..