Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 102 Linear Thermoplastic Polyurethane PEARLBOND® 102 is a linear, polycaprolactone-based polyurethane, supplied in form of small white pellets, which combines a very high crystallization rate with a very high thermoplasticity level.A.. |