Thermal Properties Metric English Comments
Softening Point 145 - 155 °C
293 - 311 °F
Oceanchem Group Brominated Epoxy Oligomers-3 (BEP-3)
Molecular Formula: (C36H32Br8O6)nCas No.: 68928-70-1Application: BEP-3 is a high molecular weight brominated epoxy polymeric flame retardant designed for a broad range of thermoplastic applications...
Softening Point 145 °C
293 °F
JIS K-2531
Unitika elitel UE3500 Polyester, Flake
High molecular weight, High toughness, High strength, High elongationUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from produc..