Softening Point 770 °C
1420 °F
Ferro EG 0026 Glaze and Sealant Glass
Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul..
Softening Point 771 °C
1420 °F
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a..
Softening Point 770 °C
1420 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott DUROBAX® amber Neutral Glass Tubing
Neutral glass tubing, chemically highly resistant, with light protection Containers, test tubes, pipettes, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, ..
Softening Point 770 °C
1420 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8326 Neutral Glass Tubing
Neutral glass tubing, alkali resistance better as for DURAN® Special lab glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is less than 100 ppm.Info..
Softening Point 770 °C
1420 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8688 Borosilicate Glass
Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium..
Softening Point 770 °C
1420 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8689 Borosilicate Glass
Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium..
Softening Point 770 °C
1420 °F
Viscosity 10<sup>7.6</sup> dPa s
Schott FIOLAX® amber Neutral Glass Tubing
Neutral glass tubing, chemically highly resistant, with light protection Pharmaceutical primary packagingInformation provided by SCHOTT AG.