Polymer Property : Softening Point = 12.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 12.0 - 150 °C
53.6 - 302 °F
Average value: 74.4 °C Grade Count:33
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Softening Point 12.0 - 20.0 °C
53.6 - 68.0 °F
Beijing Ranger Chem WAR6101 Semi Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 12.0 - 20.0 °C
53.6 - 68.0 °F
Beijing Ranger Chem E-44 Semi Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 12.0 - 20.0 °C
53.6 - 68.0 °F
Beijing Ranger Chem SM-6101 Semi Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 12.0 - 25.0 °C
53.6 - 77.0 °F
Beijing Ranger Chem SM-6101D Semi Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.