Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 114.7 °C | 238.5 °F | ETM 22-24 |
ExxonMobil ESCOREZ™ 1315 Petroleum Hydrocarbon Resin Premium aliphatic resin with a high softening point. It is a tackifying resin designed to provide high temperature performance and cohesive strength with a variety of adhesive polymers including me.. |