Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 585 °C | 1090 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
Schott Glass 8531 Soft Glass Soft glass, free from Na, of high lead content, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information provided by SCHOTT AG. |