Polymer Property : Softening Point = 101 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 101 °C
214 °F
Zeon Chemicals Quintone® C200H Aliphatic Hydrocarbon Resin
C5 type (piperylene precursor).Information provided by Zeon Chemicals L.P.
Softening Point 101 °C
214 °F
Zeon Chemicals Quintone® K100 Aliphatic Hydrocarbon Resin
C5 type (piperylene precursor). General-purpose, suitable for adhesives based on natural rubber. Better tackiness than A100.Information provided by Zeon Chemicals L.P.