Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® EX28 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | 0.250 inches; ASTM D648 |
TPI Porene® GA800TW High Gloss/Weather Resistant/Antistatic Grade ABS INJECTION MOLDING; ANTISTATIC; WEATHER RESISTANT. HOUSING OF ELECTRICAL APPLIANCES, e.g. ELECTRIC FAN, TELEPHONE, CALCULATOR, TOYSPorene® is a registered trademark of Thai Petrochemical Industry C.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C @Thickness 3.17 mm |
189 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A300 BK General Purpose (Utility) ABS Molding Resin Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | Annealed; ASTM D648 |
American Polymers API 410 Polystyrene API 410 is a low impact polystyrene with very high gloss and superior dimensional stability.Applications: API 410 is ideally suited for point of purchase displays where high gloss and some impact i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | 0.25 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3001MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | Unannealed; ASTM D648 |
Entec Hyrene® PSCRY 14 General Purpose Polystyrene Available in North America Features: General PurposeRoHS Compliant Form: Pellets Information provided by Entec |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | 0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648 |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | |
Aclo Accutech ABS ABS833G10L Glass Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | |
Aclo Accutech Polypropylene Copolymer CP0436C10L1 Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | |
Aclo Accutech Polypropylene Homopolymer HP0334G5M25CL Glass/Mineral Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | |
Aclo Acculoy PCA083L Polycarbonate ABS Alloy |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | Annealed; ASTM D648 |
American Polymers API 425 Polystyrene API 425 is a medium impact grade of polystyrene for injection molding. API 425 has good gloss, easy flow and fast cycling properties.Applications: API 425 is widely used in cosmetic packaging, food.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.2 °C | 189 °F | Unannealed; ASTM D648 |
Styron EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated.. |