Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 74.00 °C
165.2 °F
ASTM D-648
Axiall UV-7160 Rigid PVC, Molding
Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri..