Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 723 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 384 °C
723 °F
DIN 53 461
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...