Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 367 °C
693 °F
ISO 75-f
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..