Deflection Temperature at 1.8 MPa (264 psi) 68.00 °C
154.4 °F
ASTM D-648
Axiall CL-7053 Rigid PVC, Molding
Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.