Deflection Temperature at 1.8 MPa (264 psi) 66.200 °C
151.16 °F
ASTM D-648
Axiall 3101 Rigid PVC, Extrusion
Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be..