Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.00 °C
150.8 °F
unannealed; ASTM D-648
Axiall Suprel® SVA 9412 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu..