Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 559 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 293 °C
559 °F
Unannealed; Flatwise; ISO 75-2/A
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber
Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Deflection Temperature at 1.8 MPa (264 psi) 293 °C
559 °F
ISO 75; DIN 53461
Zell-Metall Engineering Plastics Zellamid 1500T (PEEK modified)
Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metall’s semi-crystalline high performance thermoplastic which exhibits a unique combination of high m..