Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 450.00 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 232.22 °C
450.00 °F
ASTM D648
Lucent Polymers G66-13 Nylon 66, 13% Glass Fiber Reinforced
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.