Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 422.1 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 216.7 °C
422.1 °F
ISO 75-1,-2
Gromax BFG50-FU00B3 Nylon 6 49.4% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Deflection Temperature at 1.8 MPa (264 psi) 216.7 °C
422.1 °F
ISO 75-1,-2
Gromax BFG50-FU00B3 Nylon 6 49.4% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.