Deflection Temperature at 1.8 MPa (264 psi) 194.44 °C
381.99 °F
ASTM D648
Lucent Polymers L6-140 Nylon 6, 15% Glass Fiber and 25% Mineral Reinforced
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.