Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 192 °C | 377 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6 Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing .. |