Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige
Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ISO 75.1
Solvay Engineered Polymers DEXFLEX® E756 TPO  (discontinued **)
Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toug..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
Spartech PP7210 Calcium Carbonate Filled High Impact Copolymer
Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LL 8450.31 Linear Low Density Polyethylene Resin
Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LLP 8450.31 Linear Low Density Polyethylene Resin
Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
Clariant 6008 L Nylon 6, High Impact, Injection Molding
Data provided by Clariant Masterbatches
Deflection Temperature at 1.8 MPa (264 psi) 37.8 - 125 °C
100 - 257 °F
Average value: 61.7 °C Grade Count:22
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..